我設計的磨砂(pmma)有機玻璃,有不對的地方,大家指正
1.磨砂有機玻璃的霧度為92%,吸收率為4%,一次性透光率為82% L`sg60z 2.我設置的有機玻璃表面參數(shù) Q7<%_a [attachment=39906] b&q!uFP 2xPkQOj3 [attachment=39907] 0r<?Ve X<:B"rPuK 3.仿真結(jié)果 ?=
G+L0t
-cDS+*[ [attachment=39908] z1dSZ0NoA 36]pE< [attachment=39909] !VLk|6mn fU/&e^,
's [attachment=39911] P{T\zT ^?+qNbK [attachment=39912] \<e? 0.pZlv [attachment=39913] U-F\3a;& u^6@!M 4.經(jīng)過有機玻璃出射的光通量 %}.4c8 MP/@Mf\<E [attachment=39914] pm2-F] HgGwV;W 我設置的面光源的總光通量為1000流明,經(jīng)有機玻璃后為418流明,可我明明設置的透光率為82%,哪里錯了,求助各位大俠。
|
|